Automatic curtain coating mirror back coating

Focus on Vacuum Metalizing Coating for 30 Years

3721A Baking Type Mirror Back Coating

This product is a glass coating mirror coating protective coating, which is applied by curtain coating. It has the characteristics of fast drying, dense film, firm adhesion, water resistance, heat and humidity resistance, and chemical corrosion resistance. The lenses produced by this product will not cause film chipping or peeling off when cutting, edging or punching.

Packaging SpecificationApplicable MaterialsApplication
25kg/drum, 250kg/drumGlassTop coat
Application MethodProduct Characteristics
Drenching (curtain coating)Fast drying, dense film, firm adhesion, water resistance, heat and humidity resistance, chemical corrosion resistance

1. Please stir thoroughly before use, then add solvent to dilute, and continue to stir until uniform. In order to eliminate air bubbles, it should be left to stand for about 0.5 hours after stirring.

2. Filter the coating with a suitable mesh filter and pour it into the paint tank.

3. A suitable mesh filter bag should be installed at the paint inlet above the knife groove of the paint spraying machine and the outlet of the return pipe to prevent dust, glass chips and other sundries from flowing into the paint knife, and at the same time partially eliminate paint bubbles.

4. During the construction process, the solvent can be added to the paint tank by dripping to keep the paint at an appropriate viscosity.

5. During the production process, the paint should be replenished in time to keep the paint tank close to full, so as to avoid the air bubbles in the backflow paint being sucked by the pump.

6. The construction viscosity of the mirror back paint is 25~50 seconds (4 cups, 23°C), the drying temperature is 140°C~180°C, the baking time is 3~10 minutes, and the dry film thickness of the film should not exceed 30μm.

7. Before stacking the mirrors, make sure they are fully dry and the temperature should drop below 35°C.

ItemIndicator
Solids content, %≥65
Fineness, um≤20
Viscosity (coated-4 cups, 23±1°C), s ≥180
Drying performance (baking temperature/baking time), (°C/ min)140-180/3-10
Construction performanceCurtain coating does not split
Adhesion (scratch spacing 1mm), class ≤1
Pencil hardness (coating scratched) ≥H
Cutting, edging, punchingNo chipping, falling off

(The products are widely used in various coated mirrors. Learn more product effects, pleaseContact Us)